主页|Alloy Steel Pipe|ASTM A671 Gr. Cc65 Cl. 12 Seamless Alloy Steel Pipe

Products on sale

ASTM A671 Gr. Cc65 Cl. 12 Seamless Alloy Steel Pipe

Categories:

    描述

    Alloy steel is alloyed with many materials including molybdenum, chromium, nickel, manganese, and a few trace elements. An Alloy Steel Pipe provides moderate corrosion resistance. These pipes are used in applications where the carbon steel pipes cannot suffice. They are designed with excellent mechanical properties. These steel alloy pipes have a tensile strength of minimum 415Mpa and yield strength of minimum 205Mpa. The ASTM A335 Pipe is a high-temperature pipe. These pipes can withstand temperatures up to 375 degrees C. They are widely used in petrochemical, oil and gas, nuclear industries, etc. 

    Alloy Steel Pipe

    Pipes and tubes are produced either seamlessly or through welding procedures. Alloy Steel Seamless Pipe is produced with the help of a single billet and without any welds. They are available in sizes of ½ to 26mm. They are very durable and easy to maintain. The Alloy Steel Welded Pipe is designed by welding pieces of steel together longitudinally. These pipes have an outer thickness of 0.3-50mm. They can be availed in a beveled or a plain end. The Seamless Alloy Steel Pipe is costlier than the welded pipe as it has 20% extra working pressure. These pipes are furthermore resistant to corrosion. The Alloy Steel ERW Pipe is manufactured by passing electricity through steel sheets. These pipes are cold-rolled to give them smooth and desired properties. Our experienced staff makes use of the best raw materials and the latest technology while producing the Alloy Steel Pipe, along with our other products.

    The Alloy Pipe Price depends on the wall thickness and the size of the pipe. An alloy pipe is available as less as 130INR per kg to 3,000INR per kg. The Boiler pipe material we used to make boiler tubes and pipes is extremely strong. These pipes suffice in temperatures up to 450 degrees C, and they don’t dissociate easily. 

     Alloy Steel Welded Pipe and ASME SA 335 Drill Pipes are suitable for High Temperature applications and boilers

    Supplier and exporter of ASTM A335 Seamless Ferritic Alloy Steel Pipes and Large size fabricated AS Pipe material in India

    ASTM A335 PIPES | ASTM A335 GR P5 PIPES | ASTM A335 GR P9 PIPES | ASTM A335 GR P11 PIPES | ASTM A335 GR P22 PIPES | ASTM A335 GR P91 PIPES
    Size Range: 1/8″ – 26″
    Schedules: 20, 30, 40, Standard (STD), Extra Heavy (XH), 80, 100, 120, 140, 160, XXH

    Alloy steel pipes are available with specifications like: ASTM A335 GR. P1/ P5/ P9/ P11/ P22/ P91 etc.

    Alloy Steel Seamless Pipe Heat Treatment

    P5, P9, P11, and P22
    Grade Heat Treatment Type Normalizing Temperature Range F [C] Subcritical Annealing 
    or Tempering 
    Temperature Range F 

    [C]
    P5 (b,c) Full or Isothermal Anneal
    Normalize and Temper ***** 1250 [675]
    Subcritical Anneal (P5c only) ***** 1325 – 1375 [715 – 745]
    P9 Full or Isothermal Anneal
    Normalize and Temper ***** 1250 [675]
    P11 Full or Isothermal Anneal
    Normalize and Temper ***** 1200 [650]
    P22 Full or Isothermal Anneal
    Normalize and Temper ***** 1250 [675]
    P91 Normalize and Temper 1900-1975 [1040 – 1080] 1350-1470 [730 – 800]
    Quench and Temper 1900-1975 [1040 – 1080] 1350-1470 [730 – 800]

    Alloy Steel Welded Pipe Chemical Requirements

    Buy MSL, ISMT, Jindal make Alloy Steel ERW Pipe at dealer price in Mumbai, check latest Low Alloy Pipe Price in India
    Seamless
    P-5 P-9 P-11 P-22 P-91 P91 shall not have a hardness not exceeding 250 HB/265 HV [25HRC].
    Tensile Strength, min., psi
    ksi 60 60 60 60 85
    MPa 415 415 415 415 585
    Yield Strength, min., psi
    ksi 30 30 30 30 60
    MPa 205 205 205 205 415

    Alloy Steel Seamless Pipe Wall Thickness

    NPS [DN] Designator Tolerance, % from Specified
    Over Under
    1/8 to 2 1/2 [6 to 65] incl., all t/D ratios 20.0% 12.5%
    Above 2 1/2  [65], t/D < or = 5% 22.5% 12.5%
    Above 2 1/2  [65], t/D > 5% 15.0% 12.5%
    (t = Specified Wall Thickness; D = Specified Outside Diameter)

    Alloy Steel Pipe Elongation

    Calculated Minimum Elongation Values
    Elongation in 2 in. or 50 mm, min %
    Wall Thickness P5, P9, P11, P22 P91
    in. mm Longitudinal Transverse Longitudinal
    5/16 (0.312) 8 30 20 20
    9/32 (0.281) 7.2 28 19 19
    1/4 (0.250) 6.4 27 18 18
    7/32 (0.219) 5.6 26 17
    3/16 (0.188) 4.8 24 16
    5/32 (0.156) 4 22 15
    7/8 (0.125) 3.2 21 14
    3/32 (0.094) 2.4 20 13
    1/18 (0.062) 1.6 18 12

    Alloy Steel Welded Pipe Outside Diameter

    Searching for Boiler Pipe suppliers in Mumbai? Distributor and stockist of Alloy Steel Seamless Pipe as per ANSI B36.19, custom length cutting service at NO EXTRA COST
    NPS [DN] Designator Over Under
    in. mm in. mm
    1/8 to 1 1/2 [6 to 40], incl. 1/64 (0.015) 0.40 1/64 (0.015) 0.40
    Over 1 1/2 to 4 [40 to 100], incl. 1/32 (0.031) 0.79 1/32 (0.031) 0.79
    Over 4 to 8 [100 to 200], incl. 1/16 (0.062) 1.59 1/32 (0.031) 0.79
    Over 8 to 12 [200 to 300], incl. 3/32 (0.093) 2.38 1/32 (0.031) 0.79
    Over 12 [300] +/- 1% of the specified outside diameter

    Seamless Alloy Steel Pipe Mechanical Tests

    Transverse or Longitudinal Tension Test and Flattening Test, Hardness Test, or Bend Test
    For material heat treated in a batch-type furnace, tests shall be made on 5% of the pipe from each treated lot.  For small lots, at least one pipe shall be tested.
    For material heat treated by the continuous process, tests shall be made on a sufficient number of pipe to constitute 5% of the lot, but in no case less than 2 pipe.
    Notes for Hardness Test: P91 shall not have a hardness not exceeding 250 HB/265 HV [25HRC].
    Notes for Bend Test: For pipe whose diameter exceeds NPS 25 and whose diameter to wall thickness ratio is 7.0 or less shall be subjected to the bend test instead of the flattening test.
    Other pipe whose diameter equals or exceeds NPS 10 may be given the bend test in place of the flattening test subject to the approval of the purchaser.
    The bend test specimens shall be bent at room temperature through 180 without cracking on the outside of the bent portion.
    The inside diameter of the bend shall be 1 inch [25 mm].
    Hydrostatic Test Each length of pipe shall be Hydro tested, at option of manufacture nondestructive electric testing can be used.

    Alloy Steel ERW Pipe price list

    SIZE” SIZE NB ALLOY STEEL A335 P5/ A213 T5 ALLOY STEEL A335 P11/ A213 T11 ALLOY STEEL A335 P22/ A213 T22 ALLOY STEEL A335 P91/ A213 T91
    1/2 15 3,970.59 1,764.71 2,058.82 5,441.18
    3/4 20 3,897.06 1,691.18 1,985.29 5,367.65
    1 25 3,823.53 1,617.65 1,911.76 5,294.12
    1.25 32 3,794.12 1,588.24 1,882.35 5,264.71
    1.5 40 3,750.00 1,544.12 1,838.24 5,220.59
    2 50 2,382.35 1,205.88 1,500.00 5,029.41
    2.5 65 2,382.35 1,205.88 1,500.00 5,029.41
    3 80 2,382.35 1,205.88 1,500.00 5,029.41
    3.5 90 2,382.35 1,205.88 1,500.00 5,029.41
    4 100 2,382.35 1,205.88 1,500.00 5,029.41
    5 125 2,382.35 1,205.88 1,500.00 5,029.41
    6 150 2,382.35 1,205.88 1,500.00 5,029.41
    8 200 2,411.76 1,235.29 1,529.41 5,058.82
    10 250 2,411.76 1,235.29 1,529.41 5,058.82
    12 300 2,411.76 1,235.29 1,529.41 5,058.82
    14 350 2,426.47 1,250.00 1,544.12 5,073.53
    16 400 2,426.47 1,250.00 1,544.12 5,073.53
    18 450 2,441.18 1,264.71 1,558.82 5,088.24
    20 500 2,441.18 1,264.71 1,558.82 5,088.24
    22 550 2,470.59 1,294.12 1,588.24 5,117.65
    24 600 2,470.59 1,294.12 1,588.24 5,117.65

    Alloying Elements

    Commonly used alloying elements and their effects are listed in the table given below.

    Alloying Elements Effect on the Properties
    Chromium Increases Resistance to corrosion   and oxidation. Increases hardenability and wear resistance. Increases high   temperature strength.
    Nickel Increases hardenability. Improves   toughness. Increases impact strength at low temperatures.
    Molybdenum Increases hardenability, high   temperature hardness, and wear resistance. Enhances the effects of other   alloying elements. Eliminate temper brittleness in steels. Increases high   temperature strength.
    Manganese Increases hardenability. Combines   with sulfur to reduce its adverse effects.
    Vanadium Increases hardenability, high   temperature hardness, and wear resistance. Improves fatigue resistance.
    Titanium Strongest carbide former. Added to   stainless steel to prevent precipitation of chromium carbide.
    Silicon Removes oxygen in steel making.   Improves toughness. Increases hardness ability
    Boron Increases hardenability. Produces   fine grain size.
    Aluminum Forms nitride in nitriding steels.   Produces fine grain size in casting. Removes oxygen in steel melting.
    Cobalt Increases heat and wear   resistance.
    Tungsten Increases hardness at elevated   temperatures. Refines grain size.